Microsection - Automatic Preparation

Product Code:DVD-29
Language:English
 
IPC Member: $289.00
Nonmember: $368.00
Add to Cart
 
 
 


DESCRIPTION

Examines the procedure for preparing microsections using automatic equipment for the critical grinding and polishing steps. Provides a thorough examination of the microsection process steps, including coupon removal, thermal stressing, mounting, grinding, polishing, and etching the specimen. Time: 29 minutes.

More about the DVD-R Format used for this product.

 
Related Products
 P-MICROP-MICRO: PCB Multi-Issue Microsection Wall Poster