OBSOLETE - SUPERSEDED BY 4204A

Product Code:4204
Language:English
 
IPC Member: $33.00
Nonmember: $65.00
Add to Cart
 
 
 


DESCRIPTION
Establishes the requirements for metal-clad dielectric film materials used in flexible printed circuitry fabrication and flexible flat cable. Provides comprehensive data that will more easily help users determine both material capability and compatibility. IPC-4204 includes the metal-clad dielectric film material specification sheets which are identified by material type. Closely aligned with IPC-4202 and IPC-4203. Supersedes IPC-FC-241C and, in turn, IPC-FC-241B, IPC-FC-241A and IPC-FC-241. 57 pages. Released May 2002.

Preview the table of contents .pdf file.

Included in the IPC-C-102 and the IPC-C-1000 Collections.

 
Related Products
 4202A4202A: Flexible Base Dielectrics for Use in Flexible Printed Circuitry